Skip to main navigation Skip to search Skip to main content

Crystalline-phase depuration in Ce3+ activated Lu3Al5O12-tellurite green-emitting phosphor-in-glass

  • D. Han
  • , D. S. Li*
  • , Y. J. Zhang
  • , H. Lin
  • , E. Y.B. Pun
  • *Corresponding author for this work
  • Dalian Polytechnic University
  • City University of Hong Kong

Research output: Contribution to journalArticlepeer-review

Abstract

Ce3+ activated Lu3Al5O12 (LuAG) phosphor-in-glass (PiG) based on tellurite glass with low melting temperature has been synthesized and the LuAG particles are proved to be well-distributed in tellurite glass with the particle size of ~5 μm. The introduction of H3BO3 as a flux is helpful to promote polycrystalline growth and reduce reaction temperature of LuAG:Ce3+ green phosphor, but accompanied by the generation of LuBO3 impurity phase. Differential fluorescence emission behaviors between LuAG:Ce3+ and LuAG-PiG illustrate that the luminous ability of the LuBO3:Ce3+ is strongly restrained while intense pure green light is released in composite. LuAG-PiG combines the admirable formability of tellurite glass with the favorable luminescent capability of LuAG:Ce3+, in which LuBO3 can be effectively eliminated to achieve LuAG:Ce3+ depuration. Prominent depuration capacity and intense fluorescence emission demonstrate that LuAG-PiG is a potential candidate in developing high-power light emitting diodes lighting.

Original languageEnglish
Article number116531
JournalJournal of Luminescence
Volume214
DOIs
StatePublished - Oct 2019
Externally publishedYes

Keywords

  • Crystalline-phase depuration
  • LuAG:Ce phosphor
  • Phosphor-in-glass

Fingerprint

Dive into the research topics of 'Crystalline-phase depuration in Ce3+ activated Lu3Al5O12-tellurite green-emitting phosphor-in-glass'. Together they form a unique fingerprint.

Cite this