Abstract
(KNa)0.1(Sr0.6Ba0.4)0.9Nb 2O6, or KNSBN, crystals have been grown with two different Mn concentrations: 0.02 wt % and 0.04 wt %. Two-wave mixing and self-pumped phase conjugation experiments were carried out on these crystals at 632.8 nm wavelength. The measured two-wave coupling gains for the 0.02 wt % and 0.04 wt % crystals are larger than 7 cm-1 and 9 cm-1, respectively, and the two-wave coupling time response is faster for the 0.4 wt % crystal. In addition, the self-pumped phase conjugation reflectivity of the 0.04 wt % crystal is measured to be as high as 70%. It is shown that the Mn dopant can increase effectively the absorption coefficient and enhance the photorefractive properties of KNSBN.
| Original language | English |
|---|---|
| Pages (from-to) | 8835-8837 |
| Number of pages | 3 |
| Journal | Journal of Applied Physics |
| Volume | 79 |
| Issue number | 11 |
| DOIs | |
| State | Published - 1 Jun 1996 |
| Externally published | Yes |
Fingerprint
Dive into the research topics of 'Growth and photorefractive properties of Mn-doped (KNa)0.1(Sr0.6Ba0.4)0.9Nb 2O6 crystals'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver