Synthesis of La-based in-situ bulk metallic glass matrix composite

  • H. Tan*
  • , Y. Zhang
  • , Y. Li
  • *Corresponding author for this work
  • National University of Singapore
  • The Singapore-MIT Alliance (SMA)

Research output: Contribution to journalArticlepeer-review

Abstract

An in-situ dendritic crystalline α-La reinforced bulk metallic glass matrix composite was successfully synthesized by chill casting a La66Al14Cu10Ni10 alloy into copper mould with a rod diameter as large as 12 mm in diameter. The critical cooling rates for the formation of the in-situ composite determined by Bridgman solidification and for complete glass formation are 15 K/s and 450 K/s respectively. The thermal stability of the residual amorphous in the composite is higher than that of the fully amorphous sample of the same alloy.

Original languageEnglish
Pages (from-to)1203-1205
Number of pages3
JournalIntermetallics
Volume10
Issue number11-12
DOIs
StatePublished - Nov 2002
Externally publishedYes

Keywords

  • A. Composites
  • B. Glasses, metallic
  • C. Casting