A number of X-, Y-, and Z-cut congruent or near-stoichiometric only Er 3+-doped or Er3+/Dn+-codoped (D n+=Mg2+, Zn2+, In3+, Yb 3+) LiNbO3 crystals were grown by the Czochralski method. The Er3+ concentrations in these crystals were determined at first from neutron activation analysis. Then, the integrated unpolarized Er 3+ absorption coefficient at the 1.5 μm wavelength region was measured as a function of Er3+ concentration in crystal. The results show that the integrated absorption coefficient (IAC) is linearly proportional to the Er3+ concentration in the crystal ([Er3+] crystal) whether the crystal is only Er3+-doped or Er 3+/Dn+-codoped, and the fitted expression is IAC=(95.0±4.6)·[Er3+]crystal for the X- or Y-cut crystals and IAC=(102.0±5.1) ·[Er3+]crystal for the Z-cut ones. These linear expressions enable to establish an optical method used to accurately determine Er3+ concentration in any only Er3+-doped or Er3+/Dn+-codoped LiNbO3 crystal from the simple and rapid unpolarized absorption measurement, and the error is within 10%.

源语言英语
页(从-至)994-996
页数3
期刊Journal of the American Ceramic Society
94
4
DOI
出版状态已出版 - 4月 2011
已对外发布

学术指纹

探究 'Concentration determination of er3+ in LiNbO3 Crystal by absorption spectroscopy' 的科研主题。它们共同构成独一无二的学术指纹。

引用此