摘要
Magnesium based Mg 9Al 1Zn 5RE (RE = Y, La, Nd, Ce, or Pr) alloys with or without an addition of 1%Si were rapidly solidified by chill block melt spinning and splat quenching. The base alloy AZ91 (Mg-9Al-1 Zn) was also rapidly solidified. Isochronal heat treatment for 1 h at 100-400°C showed that the microhardness of the ribbon maintained a similar level to that of the as spun alloy up to 300°C but decreased when heat treated at 400°C. Isothermal heat treatment for up to 24 h at 250-350°C showed that there were aging responses for the sample treated at 250°C while above this temperature, the microhardness decreased as the treatment time increased. The addition of 5% of RE elements to AZ91 displaced the Mg17Al12 phase in AZ91 with fine dispersoids of Al2RE (RE = Y or Nd) or Al11RE3 (RE = La, Nd, Ce, or Pr) in Mg-9 Al-1 Zn-5RE alloys. These Al RE intermetallics remained fine and precipitated at the grain boundaries so restraining grain growth during heat treatment at up to 400°C. Although Mg2Si precipitates were found to be present in the silicon containing alloys after heat treatment at 400°C, their size was greater than those of Al-RE intermetallics, indicating that Mg2Si has a lower thermal stability than these Al-RE intermetallics. The relationship between microhardness and grain size is discussed.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 651-661 |
| 页数 | 11 |
| 期刊 | Materials Science and Technology (United Kingdom) |
| 卷 | 12 |
| 期 | 8 |
| DOI | |
| 出版状态 | 已出版 - 8月 1996 |
| 已对外发布 | 是 |
指纹
探究 'Effect of rare earth and silicon additions on structure and properties of melt spun Mg-9Al-1Zn alloy' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver