摘要
Er3+-Yb3+ co-doped waveguide amplifiers fabricated using thermal two-step ion-exchange are demonstrated. K+-Na+ ion-exchange process was first carried out in pure KNO3 molten bath, and then field-assisted annealing (FAA) was used to make the buried waveguides. The effective buried depth is estimated to be ∼3.4 μm for the buried FAA waveguides. With the use of cut-back method, the fiber-to-guide coupling loss of ∼4.38 dB, the waveguide loss of ∼2.27 dB/cm, and Er3+ absorption loss ∼5.7 dB were measured for a ∼1.24-cm-long waveguide. Peak relative gain of ∼7.0 dB is obtained for a ∼1.24-cm-long waveguide. The potential for the fabrication of compact optical amplifiers operating in the range of 1520-1580 nm is also demonstrated.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 300-304 |
| 页数 | 5 |
| 期刊 | Optics Communications |
| 卷 | 268 |
| 期 | 2 |
| DOI | |
| 出版状态 | 已出版 - 15 12月 2006 |
| 已对外发布 | 是 |
学术指纹
探究 'Er3+-Yb3+ co-doped glass waveguide amplifiers using ion exchange and field-assisted annealing' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver