跳到主要导航 跳到搜索 跳到主要内容

Structures, properties and responses to heat treatment of Cu-Y alloys prepared by mechanical alloying

  • L. K. Tan
  • , Y. Li*
  • , S. C. Ng
  • , L. Lu
  • *此作品的通讯作者
  • National University of Singapore

科研成果: 期刊稿件文章同行评审

摘要

Cu100-xYx (x=5, 10 and 20 wt. %) alloys were synthesized from elemental powders using mechanical alloying for different durations up to 40 h. The as-milled powder samples were heat treated for 2 h at 300 and 500°C. These samples were characterized by scanning and transmission electron microscopy (SEM and TEM, respectively), X-ray diffractometry, microhardness testing and particle size analysis. Nano-sized αCu grains were found by TEM analysis in all compositions after milling for 20 h by TEM analysis. Both SEM and particle size analyzer confirmed the flattening of the particles into thin discs after milling for 2 h and their size decreased on further milling, reaching a minimum after milling for 10 h and increased significantly after milling for 20 h. No Y or secondary phases were detected by XRD for Cu95Y5 after milling for 20 h. However, a small amount of Cu5Y/Cu4Y was found in the same sample by TEM. The microhardness values increased with milling time, reaching a maximum for powder sample that had been milled for 20 h for Cu95Y5 and 40 h for Cu90Y10 and Cu80Y20 respectively. Heat treatment at 500°C for 2 h on the Cu95Y5 powders which had been milled for 20 h produced no significant coarsening of αCu grains as the size of these grains was still in the nanometer region. However, the amount of Cu5Y/Cu4Y as detected by TEM was found to increase upon heat treatment.

源语言英语
页(从-至)201-208
页数8
期刊Journal of Alloys and Compounds
278
1-2
DOI
出版状态已出版 - 1 8月 1998
已对外发布

指纹

探究 'Structures, properties and responses to heat treatment of Cu-Y alloys prepared by mechanical alloying' 的科研主题。它们共同构成独一无二的指纹。

引用此